Young's modulus of (Cu, Ag)-Sn intermetallics measured by nanoindentation

X. Deng, M. Koopman, Nikhilesh Chawla, K. K. Chawla

Research output: Contribution to journalArticlepeer-review

166 Scopus citations

Fingerprint

Dive into the research topics of 'Young's modulus of (Cu, Ag)-Sn intermetallics measured by nanoindentation'. Together they form a unique fingerprint.

Engineering & Materials Science

Physics & Astronomy

Chemical Compounds