Stress-corrosion cracking
K. Sieradzki
, R. C. Newman
Research output
:
Contribution to journal
›
Article
›
peer-review
228
Scopus citations
Overview
Fingerprint
Fingerprint
Dive into the research topics of 'Stress-corrosion cracking'. Together they form a unique fingerprint.
Sort by
Weight
Alphabetically
Physics & Astronomy
stress corrosion cracking
99%
cleavage
39%
transgranular corrosion
34%
brasses
21%
noble metals
21%
crack tips
20%
dissolving
17%
stainless steels
16%
alloying
16%
copper
13%
thin films
9%
metals
9%
Chemical Compounds
Stress Corrosion Cracking
100%
Alloy
53%
Cleavage
34%
Percolation
30%
Noble Metal
24%
Dissolution
18%
Purity
12%
Metal
11%
Engineering & Materials Science
Stress corrosion cracking
83%
Dealloying
32%
Precious metals
25%
Brass
22%
Dissolution
20%
Crack tips
19%
Thin films
17%
Stainless steel
16%
Copper
15%
Metals
12%