High porosity and surface areas of ordered mesoporous materials provide substantial capacity for loading of guest molecules, and the well-defined morphology of such materials can control their transport for controlled release. Here, the loading and release of mitoxantrone from unmodified ordered mesoporous carbon films is monitored using UV/Vis spectroscopy. Organic-organic self-assembly of Pluronic F127 with phenolic resin leads to interconnected elliptical pores (≈2 nm) in the film after carbonization. Interestingly, the total loading (2.6 ± 0.4 μg/cm2) and release of mitoxantrone is independent of film thickness (50-400 nm), suggesting diffusion limitations in pore filling. With an alternative template, the pore size increases to ≈5 nm and the mitoxantrone loading increases to 3.5 ± 0.9 μg/cm2, but the loading still remains thickness independent. Using phosphate buffered saline at 37 °C, less than 60% of the loaded mitoxantrone is readily released from the mesoporous carbon films over a two-week period. The release profile includes an initial burst with a modest fraction (<20%) of the loaded drug released within the first day, followed by a near linear release over the subsequent 5-9 days. Interestingly, the smaller pores (ca. 2 nm) release nearly 50% more mitoxantrone over 2 weeks than the larger pores (ca. 5 nm), despite the lower initial loading. These results illustrate potential limitations as well as opportunities for the use of highly hydrophobic porous materials for the controlled release of hydrophobic biologically active compounds as drug delivery systems.

Original languageEnglish (US)
Pages (from-to)143-150
Number of pages8
JournalMicroporous and Mesoporous Materials
Volume160
DOIs
StatePublished - Sep 15 2012

Fingerprint

Mitoxantrone
Carbon films
porosity
Kinetics
carbon
kinetics
UCON 50-HB-5100
drugs
Poloxamer
Phenolic resins
Mesoporous materials
phenolic resins
Carbonization
Ultraviolet spectroscopy
carbonization
Self assembly
Pore size
porous materials
Film thickness
Porous materials

Keywords

  • Controlled release
  • Drug delivery systems
  • Mesoporous carbon

ASJC Scopus subject areas

  • Materials Science(all)
  • Mechanics of Materials
  • Chemistry(all)
  • Condensed Matter Physics

Cite this

Slow release kinetics of mitoxantrone from ordered mesoporous carbon films. / Labiano, Alpha; Dai, Mingzhi; Taylor, David; Young, Wen Shiue; Epps, Thomas H.; Rege, Kaushal; Vogt, Bryan D.

In: Microporous and Mesoporous Materials, Vol. 160, 15.09.2012, p. 143-150.

Research output: Contribution to journalArticle

Labiano, Alpha ; Dai, Mingzhi ; Taylor, David ; Young, Wen Shiue ; Epps, Thomas H. ; Rege, Kaushal ; Vogt, Bryan D. / Slow release kinetics of mitoxantrone from ordered mesoporous carbon films. In: Microporous and Mesoporous Materials. 2012 ; Vol. 160. pp. 143-150.
@article{658f4caf5c44429ab3ecec62944aa587,
title = "Slow release kinetics of mitoxantrone from ordered mesoporous carbon films",
abstract = "High porosity and surface areas of ordered mesoporous materials provide substantial capacity for loading of guest molecules, and the well-defined morphology of such materials can control their transport for controlled release. Here, the loading and release of mitoxantrone from unmodified ordered mesoporous carbon films is monitored using UV/Vis spectroscopy. Organic-organic self-assembly of Pluronic F127 with phenolic resin leads to interconnected elliptical pores (≈2 nm) in the film after carbonization. Interestingly, the total loading (2.6 ± 0.4 μg/cm2) and release of mitoxantrone is independent of film thickness (50-400 nm), suggesting diffusion limitations in pore filling. With an alternative template, the pore size increases to ≈5 nm and the mitoxantrone loading increases to 3.5 ± 0.9 μg/cm2, but the loading still remains thickness independent. Using phosphate buffered saline at 37 °C, less than 60{\%} of the loaded mitoxantrone is readily released from the mesoporous carbon films over a two-week period. The release profile includes an initial burst with a modest fraction (<20{\%}) of the loaded drug released within the first day, followed by a near linear release over the subsequent 5-9 days. Interestingly, the smaller pores (ca. 2 nm) release nearly 50{\%} more mitoxantrone over 2 weeks than the larger pores (ca. 5 nm), despite the lower initial loading. These results illustrate potential limitations as well as opportunities for the use of highly hydrophobic porous materials for the controlled release of hydrophobic biologically active compounds as drug delivery systems.",
keywords = "Controlled release, Drug delivery systems, Mesoporous carbon",
author = "Alpha Labiano and Mingzhi Dai and David Taylor and Young, {Wen Shiue} and Epps, {Thomas H.} and Kaushal Rege and Vogt, {Bryan D.}",
year = "2012",
month = "9",
day = "15",
doi = "10.1016/j.micromeso.2012.05.003",
language = "English (US)",
volume = "160",
pages = "143--150",
journal = "Microporous and Mesoporous Materials",
issn = "1387-1811",
publisher = "Elsevier",

}

TY - JOUR

T1 - Slow release kinetics of mitoxantrone from ordered mesoporous carbon films

AU - Labiano, Alpha

AU - Dai, Mingzhi

AU - Taylor, David

AU - Young, Wen Shiue

AU - Epps, Thomas H.

AU - Rege, Kaushal

AU - Vogt, Bryan D.

PY - 2012/9/15

Y1 - 2012/9/15

N2 - High porosity and surface areas of ordered mesoporous materials provide substantial capacity for loading of guest molecules, and the well-defined morphology of such materials can control their transport for controlled release. Here, the loading and release of mitoxantrone from unmodified ordered mesoporous carbon films is monitored using UV/Vis spectroscopy. Organic-organic self-assembly of Pluronic F127 with phenolic resin leads to interconnected elliptical pores (≈2 nm) in the film after carbonization. Interestingly, the total loading (2.6 ± 0.4 μg/cm2) and release of mitoxantrone is independent of film thickness (50-400 nm), suggesting diffusion limitations in pore filling. With an alternative template, the pore size increases to ≈5 nm and the mitoxantrone loading increases to 3.5 ± 0.9 μg/cm2, but the loading still remains thickness independent. Using phosphate buffered saline at 37 °C, less than 60% of the loaded mitoxantrone is readily released from the mesoporous carbon films over a two-week period. The release profile includes an initial burst with a modest fraction (<20%) of the loaded drug released within the first day, followed by a near linear release over the subsequent 5-9 days. Interestingly, the smaller pores (ca. 2 nm) release nearly 50% more mitoxantrone over 2 weeks than the larger pores (ca. 5 nm), despite the lower initial loading. These results illustrate potential limitations as well as opportunities for the use of highly hydrophobic porous materials for the controlled release of hydrophobic biologically active compounds as drug delivery systems.

AB - High porosity and surface areas of ordered mesoporous materials provide substantial capacity for loading of guest molecules, and the well-defined morphology of such materials can control their transport for controlled release. Here, the loading and release of mitoxantrone from unmodified ordered mesoporous carbon films is monitored using UV/Vis spectroscopy. Organic-organic self-assembly of Pluronic F127 with phenolic resin leads to interconnected elliptical pores (≈2 nm) in the film after carbonization. Interestingly, the total loading (2.6 ± 0.4 μg/cm2) and release of mitoxantrone is independent of film thickness (50-400 nm), suggesting diffusion limitations in pore filling. With an alternative template, the pore size increases to ≈5 nm and the mitoxantrone loading increases to 3.5 ± 0.9 μg/cm2, but the loading still remains thickness independent. Using phosphate buffered saline at 37 °C, less than 60% of the loaded mitoxantrone is readily released from the mesoporous carbon films over a two-week period. The release profile includes an initial burst with a modest fraction (<20%) of the loaded drug released within the first day, followed by a near linear release over the subsequent 5-9 days. Interestingly, the smaller pores (ca. 2 nm) release nearly 50% more mitoxantrone over 2 weeks than the larger pores (ca. 5 nm), despite the lower initial loading. These results illustrate potential limitations as well as opportunities for the use of highly hydrophobic porous materials for the controlled release of hydrophobic biologically active compounds as drug delivery systems.

KW - Controlled release

KW - Drug delivery systems

KW - Mesoporous carbon

UR - http://www.scopus.com/inward/record.url?scp=84861816372&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84861816372&partnerID=8YFLogxK

U2 - 10.1016/j.micromeso.2012.05.003

DO - 10.1016/j.micromeso.2012.05.003

M3 - Article

AN - SCOPUS:84861816372

VL - 160

SP - 143

EP - 150

JO - Microporous and Mesoporous Materials

JF - Microporous and Mesoporous Materials

SN - 1387-1811

ER -