TY - JOUR
T1 - Nucleation and growth control for iron- and phosphorus-rich phases from a modified steelmaking waste slag
AU - Li, Juncheng
AU - Li, Guoxuan
AU - Qiu, Feng
AU - Wang, Rong
AU - Liang, Jinshan
AU - Zhong, Yi
AU - Guan, Dong
AU - Li, Jingwei
AU - Sridhar, Seetharaman
AU - Li, Zushu
N1 - Funding Information:
This work was supported by Jiangsu University (No. 19JDG011), the Project of the National Natural Science Foundation of China (Nos. 51874272 and 52111540265), and the Open Foundation of State Key Laboratory of Mineral Processing (No. BGRIMM-KJSKL-2022-23).
Publisher Copyright:
© 2023, University of Science and Technology Beijing.
PY - 2023/2
Y1 - 2023/2
N2 - Recovering the iron (Fe) and phosphorus (P) contained in steelmaking slags not only reduces the environmental burden caused by the accumulated slag, but also is the way to develop a circular economy and achieve sustainable development in the steel industry. We had previously found the possibility of recovering Fe and P resources, i.e., magnetite (Fe3O4) and calcium phosphate (Ca10P6O25), contained in steelmaking slags by adjusting oxygen partial pressure and adding modifier B2O3. As a fundamental study for efficiently recovering Fe and P from steelmaking slag, in this study, the crystallization behavior of the CaO—SiO2—FeO—P2O5—B2O3 melt has been observed in situ, using a confocal scanning laser microscope (CLSM). The kinetics of nucleation and growth of Fe- and P-rich phases have been calculated using a classical crystallization kinetic theory. During cooling, a Fe3O4 phase with faceted morphology was observed as the 1st precipitated phase in the isothermal interval of 1300–1150°C, while Ca10P6O25, with rod-shaped morphology, was found to be the 2nd phase to precipitate in the interval of 1150—1000°C. The crystallization abilities of Fe3O4 and Ca10P6O25 phases in the CaO—SiO2—FeO—P2O5—B2O3 melt were quantified with the index of (TU − TI)/TI (where TI represents the peak temperature of the nucleation rate and TU stands for that of growth rate), and the crystallization ability of Fe3O4 was found to be larger than that of Ca10P6O25 phase. The range of crystallization temperature for Fe3O4 and Ca10P6O25 phases was optimized subsequently. The Fe3O4 and Ca10P6O25 phases are the potential sources for ferrous feedstock and phosphate fertilizer, respectively.
AB - Recovering the iron (Fe) and phosphorus (P) contained in steelmaking slags not only reduces the environmental burden caused by the accumulated slag, but also is the way to develop a circular economy and achieve sustainable development in the steel industry. We had previously found the possibility of recovering Fe and P resources, i.e., magnetite (Fe3O4) and calcium phosphate (Ca10P6O25), contained in steelmaking slags by adjusting oxygen partial pressure and adding modifier B2O3. As a fundamental study for efficiently recovering Fe and P from steelmaking slag, in this study, the crystallization behavior of the CaO—SiO2—FeO—P2O5—B2O3 melt has been observed in situ, using a confocal scanning laser microscope (CLSM). The kinetics of nucleation and growth of Fe- and P-rich phases have been calculated using a classical crystallization kinetic theory. During cooling, a Fe3O4 phase with faceted morphology was observed as the 1st precipitated phase in the isothermal interval of 1300–1150°C, while Ca10P6O25, with rod-shaped morphology, was found to be the 2nd phase to precipitate in the interval of 1150—1000°C. The crystallization abilities of Fe3O4 and Ca10P6O25 phases in the CaO—SiO2—FeO—P2O5—B2O3 melt were quantified with the index of (TU − TI)/TI (where TI represents the peak temperature of the nucleation rate and TU stands for that of growth rate), and the crystallization ability of Fe3O4 was found to be larger than that of Ca10P6O25 phase. The range of crystallization temperature for Fe3O4 and Ca10P6O25 phases was optimized subsequently. The Fe3O4 and Ca10P6O25 phases are the potential sources for ferrous feedstock and phosphate fertilizer, respectively.
KW - calcium phosphate
KW - growth
KW - kinetics
KW - magnetite
KW - nucleation
KW - steelmaking slag
UR - http://www.scopus.com/inward/record.url?scp=85142458839&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=85142458839&partnerID=8YFLogxK
U2 - 10.1007/s12613-022-2553-x
DO - 10.1007/s12613-022-2553-x
M3 - Article
AN - SCOPUS:85142458839
SN - 1674-4799
VL - 30
SP - 378
EP - 387
JO - International Journal of Minerals, Metallurgy and Materials
JF - International Journal of Minerals, Metallurgy and Materials
IS - 2
ER -