Molecular dynamics simulation of high-speed nanoindentation

Hualiang Yu, James Adams, Louis G. Hector

Research output: Contribution to journalArticlepeer-review

27 Scopus citations

Fingerprint

Dive into the research topics of 'Molecular dynamics simulation of high-speed nanoindentation'. Together they form a unique fingerprint.