Electrochemical aspects of stress-corrosion cracking of sensitised stainless steels

R. C. Newman, K. Sieradzki

Research output: Contribution to journalArticlepeer-review

35 Scopus citations

Fingerprint Dive into the research topics of 'Electrochemical aspects of stress-corrosion cracking of sensitised stainless steels'. Together they form a unique fingerprint.

Chemical Compounds

Engineering & Materials Science