Combined AFM Nanoindentation and Finite Element Analysis of Soft Heterogeneous Biomaterials

Bryant L. Doss, Jack Rory Staunton, Melanie Dannemeyer, Mark Linhart, Robert Ros

Research output: Contribution to journalArticle

1 Scopus citations
Original languageEnglish (US)
Pages (from-to)866-867
Number of pages2
JournalMicroscopy and Microanalysis
Volume18
Issue numberS2
DOIs
Publication statusPublished - 2012

    Fingerprint

ASJC Scopus subject areas

  • Instrumentation

Cite this